Abstract The creep test of Sn-0.5 Wt.% Zn and Sn-9 Wt.% Zn alloys has been studied at different temperatures from 373 K to 453 K and under different applied stresses ranging from 12.4 MPa to 16.2 MPa. The low Zinc concentration alloy shows a transition point at 413 K, while the high Zn concentration alloy shows a transition point at 423 K. |